Industrial
Aug 15, 2013
20
Had some scaffold boards that got hot enough during PWHT to smolder and possibly have an open flame. Boards were put out buy water hose. If I were to do hardness test on this pipe is there a specific way or layout of the test on the pipe?
 
Replies continue below

Recommended for you

try to use a grid with a spacing 25mm for each hardness measurement . This hardness test can be performed by a portable hardness reader.
 