Dear and Respected,
We are performing hardness testing of field sour line piping joints. Is it possible to take hardness of weld cap? Our WPS got qualified with hardness of 225(Vicker). Our project requirement is 248max. Now the scenario is for weld joint hardness value come around 262 and in HAZ it comes around 195. I think this much difference is not possible. I read some where that in field weld cap hardness measurement is not possible due to irregular surface. Can you please guide? And what are the requirements in actual. To verify the PWHT and for other sour lines below 19mm do we need the hardness of HAZ and base metal or all three the weld metal , haz and base metal.
We are performing hardness testing of field sour line piping joints. Is it possible to take hardness of weld cap? Our WPS got qualified with hardness of 225(Vicker). Our project requirement is 248max. Now the scenario is for weld joint hardness value come around 262 and in HAZ it comes around 195. I think this much difference is not possible. I read some where that in field weld cap hardness measurement is not possible due to irregular surface. Can you please guide? And what are the requirements in actual. To verify the PWHT and for other sour lines below 19mm do we need the hardness of HAZ and base metal or all three the weld metal , haz and base metal.