Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Have a Application for ASTM 516 Grade Plate vs 4130 Round

Status
Not open for further replies.

Butch1946

Industrial
Dec 19, 2013
4
I have an application that uses ASTM 516, Grade 70 Plate. I can get it flamed cut to the sizes I need, but for large quantities, it is very expensive. Is there an alternative material I can use. Say the likes of 4130 Material in round bars. Would be cost effective if this were possible
 
Replies continue below

Recommended for you

That certainly is one option. Difficult to give you any further advice without knowing anything about the end use, etc.

 