Jun 8, 2011 #1 magee913 Civil/Environmental Mar 12, 2011 3 0 0 US can anybody point me into the right direction of how to estimate the maximum temperature experienced during curing?
can anybody point me into the right direction of how to estimate the maximum temperature experienced during curing?
Jun 8, 2011 #2 concretemasonry Structural Nov 29, 2006 1,781 0 0 US What size of concrete pour? What type of cement (Type I or Type III Portland) and what pozzolanics/ash and admixtures? Temperature of the concrete when placed? Method and time of curing? Too many different factors for a one sentence question. Dick Engineer and international traveler interested in construction techniques, problems and proper design. Upvote 0 Downvote
What size of concrete pour? What type of cement (Type I or Type III Portland) and what pozzolanics/ash and admixtures? Temperature of the concrete when placed? Method and time of curing? Too many different factors for a one sentence question. Dick Engineer and international traveler interested in construction techniques, problems and proper design.
Jul 14, 2011 1 #3 ajose Structural May 23, 2003 54 0 0 VE There is a description with explanation on EM 1110-2-542 Engineering and design. Thermal Studies of mass concrete structures. USACE (free internet download) ACI 207.1 Mass concrete (here it is a simple method proposed by Schmidt) Like concretemasonry and you can verify with this references, temperature goes over many factors ajose Upvote 0 Downvote
There is a description with explanation on EM 1110-2-542 Engineering and design. Thermal Studies of mass concrete structures. USACE (free internet download) ACI 207.1 Mass concrete (here it is a simple method proposed by Schmidt) Like concretemasonry and you can verify with this references, temperature goes over many factors ajose