Jun 21, 2011 #1 petedie Mechanical Feb 23, 2007 23 0 0 CA Hello, I have an application where I need to heat a rotating disc to ~100C. The unit is hand held similar to a pizza cutter... I appreciate any/all ideas Pete
Hello, I have an application where I need to heat a rotating disc to ~100C. The unit is hand held similar to a pizza cutter... I appreciate any/all ideas Pete
Jun 21, 2011 #2 asimpson Mechanical Aug 6, 2010 300 0 0 IE Induction heating, if disk ferromanetic. See miniductor on web Or hot air gun Upvote 0 Downvote
Jun 21, 2011 #3 M MintJulep Mechanical Jun 12, 2003 9,810 1 38 JP Direct flame impingement. Upvote 0 Downvote
Jun 21, 2011 #4 IRstuff Aerospace Jun 3, 2002 44,376 6 38 US Or infrared heaters Is that the only requirement? Otherwise, how about a Bunsen burner? Uniformity? Latency? Limits on overheat? TTFN FAQ731-376 Chinese prisoner wins Nobel Peace Prize Upvote 0 Downvote
Or infrared heaters Is that the only requirement? Otherwise, how about a Bunsen burner? Uniformity? Latency? Limits on overheat? TTFN FAQ731-376 Chinese prisoner wins Nobel Peace Prize
Jun 21, 2011 #5 GregLocock Automotive Apr 10, 2001 23,133 3 38 Orbiting a small yellow star Pour cooking oil over it. Cheers Greg Locock New here? Try reading these, they might help FAQ731-376 http://eng-tips.com/market.cfm? Upvote 0 Downvote
Pour cooking oil over it. Cheers Greg Locock New here? Try reading these, they might help FAQ731-376 http://eng-tips.com/market.cfm?
Jun 22, 2011 #6 gruntguru Mechanical Mar 1, 2008 1,247 0 36 AU Mount a brake caliper and use friction. Engineering is the art of creating things you need, from things you can get. Upvote 0 Downvote
Mount a brake caliper and use friction. Engineering is the art of creating things you need, from things you can get.
Jun 22, 2011 Thread starter #7 petedie Mechanical Feb 23, 2007 23 0 0 CA Interesting ideas, but I need to melt/fuse vinyl gaskets together (corners, additional sections). I can't find anyone out there that sells this stuff so I need to make our own... Infra red heater is a neat, clean idea... Pete Upvote 0 Downvote
Interesting ideas, but I need to melt/fuse vinyl gaskets together (corners, additional sections). I can't find anyone out there that sells this stuff so I need to make our own... Infra red heater is a neat, clean idea... Pete