Ehman316
Petroleum
- Jul 15, 2016
- 1
Hello,
I'm trying to find the best bolt/stud material used for offshore cranes. ASTM 320/320M. Only exception they note on API-2C spec is the minimum average impact energy obtained from a set of three tests shall be 30 ft-lb. (40.6 Joules) with no single test value less than 22 ft-lb. (29.8 Joules). Test temperature shall be the lower of 0°F (−17.8°C) or 10°F below the lowest design service temperature.
Would L7M be sufficient for this testing?
Thanks
I'm trying to find the best bolt/stud material used for offshore cranes. ASTM 320/320M. Only exception they note on API-2C spec is the minimum average impact energy obtained from a set of three tests shall be 30 ft-lb. (40.6 Joules) with no single test value less than 22 ft-lb. (29.8 Joules). Test temperature shall be the lower of 0°F (−17.8°C) or 10°F below the lowest design service temperature.
Would L7M be sufficient for this testing?
Thanks