Nov 2, 2012 #1 JKALLPA Mechanical Oct 2, 2012 12 0 0 AR I'd like to know about experiences on gas turbines with this kind of filters. Regards, JC
Jan 15, 2013 #2 dinadores Electrical Jan 15, 2013 1 0 0 EG i have this kind installed at SIEMENS SGT-300 and SGT-400 it is good but it should be replaced every 10 months may be due to the site is near to the sea, but we are suffering from replacing it every few months. Upvote 0 Downvote
i have this kind installed at SIEMENS SGT-300 and SGT-400 it is good but it should be replaced every 10 months may be due to the site is near to the sea, but we are suffering from replacing it every few months.
Jan 15, 2013 Thread starter #3 JKALLPA Mechanical Oct 2, 2012 12 0 0 AR What about your prefilters? What's your type of environment? Upvote 0 Downvote
Jan 16, 2013 #4 rmw Mechanical Feb 6, 2002 5,724 0 0 US Dinadores, Do you get any indication of salt pass-through with this filter? rmw Upvote 0 Downvote