Hadiabdollahi

Materials
May 24, 2018
11
Hi Dear
I am Hadi and have a quation as follow
We need some LWN flange Astm A 105. We making this flang from forged round bar. And machenical test were down and result in passed astm a 105 machenical requierment, composition test, too. So pls let me to know is have any way to marking them with Astm A 105 and Asme B16.5. If Not, help me wich kind of standard can cover this issue
 
Replies continue below

Recommended for you

Are the standard made to the requirements of ASME B16.5? If so, review B16.5 chapter 4.
 
One further advice I shall give you, based on your questions; read the standard. If you don’t have it at hand, buy a copy. The standards contain answers to most questions usually, whereas members of this site are not paid for giving advice. If you need advice, better come up with good questions.
 
You should also most likely be looking at ASME SA-105 rather than ASTM A-105.

Regards,

Mike