[smile]Hi all;

I have difficuties in finding information to solve following practical situation.

How to calculate corrosion rate of AC HK alloy in air at 1600 F running for a 100 hrs test period?
I would appreciated any help.
 
What is AC HK Alloy?
 
What is the corrosion medium? Air?
 
Hi
Thanks for your replies. I believe AC HK alloy is HK40 which is Cr/Ni high temperature resistance alloy. It has been using reformer tubes in Hydrogen furnaces in refineries. The medium is AIR.

RELATED SPECIFICATIONS
ASTM: A 297 (HK); A 351(HK30 and HK40); A 567 (HK40 and HK50 - specification discontinued in 1987); A608
(HK30 and HK40)
Nearest wrought grade: AISI 310.

Thanks
 
The oxidation rate in air is less than 0.010 inches (0.1 mm) per year.
 
Thanks Stanweld. Can you tell me how did you come to this number? I mean calculations steps.

[wavey2]

 
You should be doing your homework yourself.

NX 7.5.5.4 with Teamcenter 8 on win7 64
Intel Xeon @3.2GHz
8GB RAM
Nvidia Quadro 2000
 
The information is in published literature, in the Metals Handbook and other sources. It is based on empirical measurements - not on calculations.
 
Thanks
 
There is at least one Nickel Development Institute publication covering this. Just google them.
 
If it is homework use air.

If it is real world, find out what the composition of the air axctually is.

Thomas J. Walz
Carbide Processors, Inc.

Good engineering starts with a Grainger Catalog.
 
If your concern is the corrosion rate calculation for high temperature oxidation, please find the Air Corrosion Nomograph of Fe-Ni-Cr alloys in “Corrosion Engineering” by Fontana.