If you have hot air staking with glasfiber reinforced PET plastic against steel. Do you guys think it will be a problem with the termal expansion, if the temperature will raise up to 140 degree celcius, since the plastic will be glued to the steel sheet, which should create a shear force?

The termal expansion of the plastic will be 24 and for the steel 12
 