hot tap welding procedures

Status
Not open for further replies.

rmx8004

Petroleum
May 7, 2008
5
Does anyone know if a hot tap requires its own welding procedure. I.e does a mockup need to be made, and does it need to pass the ASME IX bend tests.

Or does a qualified welding procedure for the material being welded suffice (i.e a normal fabrication WPS)
 
Replies continue below

Recommended for you

rmx..

"Hot tapping" is an activity that is commonly contracted to experienced contractors who have thier own approved welding proceedures.

Unlike most of the goofy ASME code rules and "Nonmandatory Appendices", the API RP 2201 recommended practice is a complete document that addresses this question.

-MJC

 