Hot Working of 25CrMo4 Steel with Tellurium Additions

Status
Not open for further replies.

jimsan

Industrial
Aug 12, 2003
26
Tellurium is added to steels to modify the inclusions and improve machinability.
Does anyone have any experience of hot working such materials (25CrMo4 for example) and experienced cracking problems?
 
Replies continue below

Recommended for you

We regularly hot-head 25CrMo4 bolt heads with no cracking, but I didn't know Tellurium was an element added deliberately. To what spec ?
 