The object is the indenting ball for a hardness tester. Can the ball be picked up with an ordinary magnet? Thanks!
 
Replies continue below

Recommended for you

The tungsten carbide isn't magnetic, but the 3 to 20%Cobalt in the mixture is ferromagnetic, like iron or nickel. So how it responds to a magnetic field depends mostly on the ratio of cobalt to WC.
 
The test method for the magnetic permeabilty of cemented carbides is ASTM A342.
 