Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to check elongation on SMA wire during tensile?

Status
Not open for further replies.

hexa2016

Mechanical
Sep 19, 2016
26
hi,

how can i check elongation/strain on SMA wire during tensile?


Thanks
 
Replies continue below

Recommended for you

Like you would any wire?
Most wire people put ink marks on the wire or small tape flags and then measure elongation with optical trackers.
I have done this with wire that only had 0.5% elongation at fracture.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Not the old units, but I presume that the technology has improved significantly.
You might need to talk to optical guys that are not in the testing business, but I am sure that it can be done.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Strain gauges use the change in electrical resistance of wire to measure strain. You have a wire, so ...
 
Contact your local testing lab.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 