I need help on abobe mentioned topic. for example material is sa-516gr710 Normalized and MDMT=-45°C. How to determine required impact test energy.
 
Replies continue below

Recommended for you

SA-516-70 has min specified yield strenght of 260 Mpa. So for a 50 mm plate, required Cv=20J. am I right? please clarify
 