Mechanical
Sep 11, 2006
67
I have three questions.

1.Does 'glass-lined' mean 'fiberglass-reinforced Plastics(FRP)'?

2.Are there standards or codes about FRP for pressure equipments?

3.How to inspect a glass-lined pressure equipment effectively?

Thanks in advance.
 
Replies continue below

Recommended for you

1.Does 'glass-lined' mean 'fiberglass-reinforced Plastics(FRP)'?
No. "Glass lined" literally means lined with glass. Glass is sprayed on the vessel steel and baked in a furnace to fuse the glass on the steel.

2.Are there standards or codes about FRP for pressure equipments?
Yes. One such code is ASME Section X.



 
3.How to inspect a glass-lined pressure equipment effectively?

Start with spark testing to ensure the integrity of the glass. Contact the equipment manufacturer (I would guess it's either Pfaudler or Dd Dietrich)for more information, including testing equipment and procedures.
 