Dec 9, 2008 #1 Best99 Materials Sep 22, 2008 17 0 0 TH Dear sirs, Please suggest me about standard or equipment that appropriate for coil spring 's roughness measurement. Thank you for all kind support
Dear sirs, Please suggest me about standard or equipment that appropriate for coil spring 's roughness measurement. Thank you for all kind support
Dec 9, 2008 1 #2 CoryPad Materials Apr 15, 2002 5,192 0 0 US Here are some suitable instruments: http://veeco.com/Products/metrology_and_instrumentation/Stylus_Profilers/index.aspx http://www.mitutoyo.com/ProductTypeResultForm.aspx?type=1148 http://www.zeiss.com/imt(look for Contourecord and Surfcom) Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
Here are some suitable instruments: http://veeco.com/Products/metrology_and_instrumentation/Stylus_Profilers/index.aspx http://www.mitutoyo.com/ProductTypeResultForm.aspx?type=1148 http://www.zeiss.com/imt(look for Contourecord and Surfcom) Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.