How to passivate existing Stainless steel pipe work

Status
Not open for further replies.

Andyfish

Industrial
Nov 25, 2009
1
I have a Demineralised water plant and have corrosion in the pipe work . Is there a flushing process that will passivate the ring main that can be done retrospectivly
 
Replies continue below

Recommended for you

We follow ASTM A967 for field passivation of pipe and tubing.
 