How to predict the ferrite content in the 9%Cr-1%Mo steel (P91) ?

Status
Not open for further replies.

stanislasdz

Materials
Jan 20, 2007
250
How to predict the ferrite content in the 9%Cr-1%Mo steel (P91)

Thanks

 
Replies continue below

Recommended for you

stanislasdz;
You can predict ferrite content by obtaining a CCT diagram for this steel. They are available. You can also contact V&M for this information.
 
stanislasdz;
Looks interesting and I will read the paper. I would still contact V&M because they have been producing Grade 91 material for years. They would be very helpful in this area.
 