Power_Plant_Matt
Nuclear
- Oct 31, 2019
- 2
I have a battery bank with about 100 cells that are linked together using 1/4" x 3" x 8" aluminum bars. Maintenance and I have been trying to figure out what the "appropriate" amount of No-Ox would be to apply on the links, posts, and connection points and also how to apply it (paint brush, paper towel, rubber glove, wipe off excess, leave on excess). It seems like it should be a no-brainer, but we've actually had quite a long conversation about it. The environment is clean, dry, temperature controlled to around 70F, and indoors. Any tips? I attached some photos for reference.
This one has more grease
This one has less grease
This one has more grease
This one has less grease