We are being contracted to fabricate an austenitic(316) pipe in pipe lance feeding a dual liquid nozzle(air and steam). Process pressures are 80psi. 80 psi in the inner pipe and 80 psi in the outer pipe. Lance will be operated in a duct exposed to 1400°F gas temp. Typically we receive only process pressures and temperatures. If one was to use B31.3 Paragraph 345.4.2 Test Pressure to determine hydro test pressure. In this case St/S exceeds the allowable 6.5...what does one do when this happens? If I do the calculation using the process info the ratio equals 8.7 and the hdro pressure equals 1069 psi. Any help would be appreciated.