I am dealing with an MTR for pipe from COMCO supplier. There is confusion about the associated heat numbers. The mill has provided several MTR's with identical heat numbers showing up in separate MTR's each having slightly different compositions for both product and heat analysis. Also in the MTR are additional heat numbers that are not relevant to our tag number for the PO.
So I have two questions:
1) If the heat number traces the original cast (heat) or roll (product), how can the composition vary? For instance, wt.% carbon for heat # X = 0.13 in MTR2, and wt.% carbon for heat # X = 0.15 on MTR3. Is there an acceptable variance I should be aware of according to a standard or rule of thumb.
2) Does the mill provide multiple MTR's for the same heat number to represent different sections of pipe?
Thank you!
So I have two questions:
1) If the heat number traces the original cast (heat) or roll (product), how can the composition vary? For instance, wt.% carbon for heat # X = 0.13 in MTR2, and wt.% carbon for heat # X = 0.15 on MTR3. Is there an acceptable variance I should be aware of according to a standard or rule of thumb.
2) Does the mill provide multiple MTR's for the same heat number to represent different sections of pipe?
Thank you!