Identify ASTM SA 387 GR D 1969

Status
Not open for further replies.

irx

Mechanical
Jan 30, 2007
6
Hi Everbody

A client mentioned this material ASTM SA 387 GR D - the fabrication was done in 1969. Does anybody know what is the modern equivalent of this material? Is it similar to P11 or P22? I can not find any reference in ASME II.

Thanks

IRX
 
Replies continue below

Recommended for you

I don't have ASME Section II at hand. All I know is back in the early 70's, the designation of SA 387 grades were changed from alphabetic to numeric. Grades were changed as...
Gr. B = Gr. 12
Gr. C = Gr. 11
Gr. D = Gr. 22
Gr. E = Gr. 21
 
Gentlemen

Thank you to both Kenvlach and Doct9960 you gave me exactly what I was looking for

Thanks again

IRX

 