Chromium 3.27
Carbon 0.41
Molybdenmum 0.96
Manganese 0.54

Ni .22, Si .21, V .19, Cu .25, Al .02
Remainder is iron

What is this grade? I have looked through all my referrence books, no luck with the chromium content.

Thanks in advance
 
Replies continue below

Recommended for you

Steve898;
What is the function of the steel component with this composition? This would help.
 