We are going fabricate a SS316L/SS310 vessel with MDMT= -300F using GTAW and SAW. The vessel meets the requirements of UHA-51(g), stress ratio less than 0.35.
First clarification: Per UHA-51(g) the base metal, WPS and production welds do not need to be qualified by impact testing but do the welding consumables still required to be pre-use impact tested per UHA-51(f)?
Second: Does UHA-51(f)(2) require the use of impact qualified WPS in production? Figure JJ-1.2-3 seems to imply that this is a requirement.
Any insight would be appreciated.
Thank you
First clarification: Per UHA-51(g) the base metal, WPS and production welds do not need to be qualified by impact testing but do the welding consumables still required to be pre-use impact tested per UHA-51(f)?
Second: Does UHA-51(f)(2) require the use of impact qualified WPS in production? Figure JJ-1.2-3 seems to imply that this is a requirement.
Any insight would be appreciated.
Thank you