Angsi2
Mechanical
- Oct 21, 2007
- 27
Are there any restrictions on pipe/schedule sizes below which specimen and satisfactory impact testing cound not be performed? ASTM A370 does not provide any guidelines on this.
The smallest specimen per A370 is 2.5mm x 10mm x 50mm.
Any input will be appreciated.
The smallest specimen per A370 is 2.5mm x 10mm x 50mm.
Any input will be appreciated.