In the March, 2019 AWS Welding Journal page 44 the following: 'Investigation of a Ruptured
Socket Weld in Sour Service'. Very interesting. It looks like they welded a weld neck flange
into a SW valve? The SW was a single pass?. 'Table 4'? I have some questions but thought I would just throw this article out there for comments.
 
Replies continue below

Recommended for you

A link to this article would be useful, as a starters. Otherwise, those not subscripted to the AWS Welding Journal dont have an idea what youre talking about.
 