Inconel 725

Status
Not open for further replies.

metalonis

Mechanical
Feb 28, 2002
183
Is there a corresponding Harmonised Standard number for Inconel 725 (UNS N07725) bar?
 
Replies continue below

Recommended for you

As far as I know the only specs that it appears in are ASTM B805 and ISO 18274

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
ASTM B805, ASME Code Case 2217, Special Metals Corp. specification -HA91
 