timsch
Mechanical
- Oct 27, 2009
- 191
I am trying to find the allowable stress value for Inconel 800H @ -49F. For ferrous materials, there is General Note (e) for table 1A in II-D.
"(e) Stress values for -20°F to 100°F are applicable for colder temperatures when the toughness requirements of Section III,VIII, or XII are met."
I don't see a corresponding note for Table 1B. I'd assume that the same would apply, in that impact testing is required, and the same rules would apply, where the allowable stress from -20 - 100F is used.
Where do I find info on this?
"(e) Stress values for -20°F to 100°F are applicable for colder temperatures when the toughness requirements of Section III,VIII, or XII are met."
I don't see a corresponding note for Table 1B. I'd assume that the same would apply, in that impact testing is required, and the same rules would apply, where the allowable stress from -20 - 100F is used.
Where do I find info on this?