mfgenggear
Aerospace
- Jan 23, 2008
- 3,119
Spline Shaft with external spline.
Material AISI 9310 core hardness 33-43 HRc
External Spline is carburized to 58 min HRc hardness
case depth .018-.025
I want to a run a test with one part that has been carburized, Harden & tempered.
I want to see if this would be a viable repair or am I
chasing up a tree.
I want to Induction anneal the spine area dead soft.
Then I want to Induction harden & temper the spline.
then I want to cut the ahaft down the middle and run hardness test verifing the core & case.
question ? would be it possible to maintain the core & case hardness, and the martensite properties?
can a transition/heat affected zone be prevented.
Please advise
Thanks in Advance
Material AISI 9310 core hardness 33-43 HRc
External Spline is carburized to 58 min HRc hardness
case depth .018-.025
I want to a run a test with one part that has been carburized, Harden & tempered.
I want to see if this would be a viable repair or am I
chasing up a tree.
I want to Induction anneal the spine area dead soft.
Then I want to Induction harden & temper the spline.
then I want to cut the ahaft down the middle and run hardness test verifing the core & case.
question ? would be it possible to maintain the core & case hardness, and the martensite properties?
can a transition/heat affected zone be prevented.
Please advise
Thanks in Advance