Materials
Feb 5, 2013
7
What is your opinion about MASTERSEAL SP120 & HDPE can those materials be successfully used as a internal coating/lining material for concrete based tanks subjected to the acidic waste water. Waste water has following ingredients concentration: Cadmium (0.00087); Chlorine (12.3); Chromium (0.048); Copper (0.032); Iron (2.0); Lead (0.0093); Manganese (0.069); Nickel (0.054); Sulphate (182); TSS (55.4); TDS (216); Zinc (2.2); pH = 3....respective concentarions are expresed in ppm.
Also other suggestions about suitable materials would be greatly appreciated.

Thanks

 
Replies continue below

Recommended for you

The suitability of this coating will depend on the application which you have stated. What is the application?
 
It's temporary waste water collecting basin. But lets say in a worse case scenario, if the tank is for permanent storage, what would be better a solution in a case of long term contact.

Thanks
 