Is ASTM A105 compatible with Jet A1 fuel? 1

Status
Not open for further replies.

mzappett

Mechanical
Aug 4, 2005
5
Hi all,
I am trying to find informations about the compatibility of ASTM A 105 N (and other carbon steel like LF2, F60, etc...) with aviation fuel, especially with Jet A1 class.
Bets regards

Massimo
--
Ing. Massimo Zappettini
VIAR Valvole
Technical Dept.

 
Replies continue below

Recommended for you

Hello Mr. Zappettini;

I am not aware of any problems related to using carbon steel piping for refined fuels. Carbon steel line piping (API 5L) is used for cross country pipelines that carry all types of refined fuels.

Best regards - Al
 