metalhoosier
Materials
- Nov 27, 2007
- 29
Can Code Case 2235-9 - Use of Ultrasonic Examination in Lieu of Radiography Section I; Section VIII‚ Divisions 1 and 2; and Section XII be used for B31.1 pressure piping? My first answer is obviously no based on the criteria called out in the title of the code case, however, a contracted NDE firm has claimed they have used this code case for B31.3 and was curious if and where a loophole exists to extend this NDE to other code sections.
Thank you,
MetalHoo
Thank you,
MetalHoo