As per Cl. 5.5.6.1.d of ASME Sec. VIII Div 2,
"The allowable limit on the primary plus secondary stress range, Sps, is computed as the larger of the quantities shown below.
1) Three times the average of the S values for the material at the HIGHEST & LOWEST temperatures during the operational cycle.
2) Two times the average of the Sy values for the material at the HIGHEST & LOWEST temperatures during the operational cycle."
My query is,
In above allowable stress calculation, is it correct to take AMBIENT temperature as LOWEST temperature, if lowest operating temperature is not defined?
Or Can I take Design Temperature as LOWEST as well as HIGHEST temperature in such case.
Thanks in advance
"The allowable limit on the primary plus secondary stress range, Sps, is computed as the larger of the quantities shown below.
1) Three times the average of the S values for the material at the HIGHEST & LOWEST temperatures during the operational cycle.
2) Two times the average of the Sy values for the material at the HIGHEST & LOWEST temperatures during the operational cycle."
My query is,
In above allowable stress calculation, is it correct to take AMBIENT temperature as LOWEST temperature, if lowest operating temperature is not defined?
Or Can I take Design Temperature as LOWEST as well as HIGHEST temperature in such case.
Thanks in advance