Mar 6, 2008 #1 etsen Mechanical Joined Sep 11, 2006 Messages 67 Location CN SA 240 TP 347 is used in internal cone of a heat exchanger. I think SA240 TP347 is wrong, because I can not find SA240 TP347 in the ASME BPVC SEC II - PART A. But I am not sure whether it is right. Could anybody explain that? Thanks a lot.
SA 240 TP 347 is used in internal cone of a heat exchanger. I think SA240 TP347 is wrong, because I can not find SA240 TP347 in the ASME BPVC SEC II - PART A. But I am not sure whether it is right. Could anybody explain that? Thanks a lot.
Mar 6, 2008 #2 TGS4 Mechanical Joined Nov 8, 2004 Messages 3,992 Location CA It's there - keep looking. Upvote 0 Downvote
Mar 6, 2008 1 #3 doct9960 Mechanical Joined Aug 15, 2006 Messages 618 Location CA SA-240 is a plate specification. Drop the term "TP" on the grade designation. "TP" applies to tubular products (tubes & pipes) Upvote 0 Downvote
SA-240 is a plate specification. Drop the term "TP" on the grade designation. "TP" applies to tubular products (tubes & pipes)
Mar 6, 2008 1 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US People confuse Type with "TP" thinking that it is an abbreviation of Type. SA 240 Type 347 is there. Upvote 0 Downvote