t2photo
Materials
- Dec 12, 2008
- 4
hi every one i was told that 4140 should never be used past a hardness of 42 Rockwell max is this true? we have been using this matrial at 48-52roc for quite awhile and havent had a problem till reciently the pieces just shattered with not much force and this particular part could cause some major acident if it failed at the wrong time. any help or ideas are greatly appreciated.