Hi there
I have a particular application where the compression of my part induces stresses WAY beyond the yield stress. The small amount of elasticity remaining in the part is fundamental to the design as it has to survive approx one million cycles of +/- 20 microns. Unfortunately on the current design cracks are appearing and we need to somehow improve it. The part has a section of only a few mm, is made from stainless-steel and the compression is across the section NOT along the length.
My question is can fatigue calculation software model this kind of fatigue problem with high plasticity, low strain cycling and a million cycles? I'm looking at packages like MSC.Fatigue as we already have an account with them.
Any help or advice on my problem is appreciated.
Thanks in advance
Zatt.
I have a particular application where the compression of my part induces stresses WAY beyond the yield stress. The small amount of elasticity remaining in the part is fundamental to the design as it has to survive approx one million cycles of +/- 20 microns. Unfortunately on the current design cracks are appearing and we need to somehow improve it. The part has a section of only a few mm, is made from stainless-steel and the compression is across the section NOT along the length.
My question is can fatigue calculation software model this kind of fatigue problem with high plasticity, low strain cycling and a million cycles? I'm looking at packages like MSC.Fatigue as we already have an account with them.
Any help or advice on my problem is appreciated.
Thanks in advance
Zatt.