Hi Guys,

I'm trying to find out what kind of isolation(shut off) valves are commonly used in hydrometallurgical processes. I can only find information on throttling valves, but I can't imagine that there are nog isolation valves, espacially when acid or other chemicals are used. Anyone who can help?

Cheers, Roy
 
Isolation valves are normally knifegate valves of a non-corosive material.

Contact in Canada, probably other links attached
or clarkson
 