Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

JIS H3250 brass

Status
Not open for further replies.

clarko6

Materials
Nov 18, 2010
1
Is JIS H3250 brass the same as C2600 or C26000 brass. I have some terminals mfg overseas and first they tell me that C2600 is the same as C26000, but then also reference the JIS H3250 as material used.
What gives?
 
Replies continue below

Recommended for you

JIS H3250 is a standard for copper & copper alloy rods and bars which then references a number of different grades (chemical composition, properties, etc.) such as C 2600. In North America, ASTM B927/927M is the standard for brass rod, bars and shapes, and UNS C26000 is one of the grades referenced therein.
 