Dec 16, 2004 #1 soya Mechanical Dec 9, 2004 11 0 0 GB Dear friends, Could anyone let me know how to get the Jominy Test data(eg the position of the specimen and the response temperature together with the time)? Thanks.
Dear friends, Could anyone let me know how to get the Jominy Test data(eg the position of the specimen and the response temperature together with the time)? Thanks.
Dec 16, 2004 #2 EdStainless Materials May 20, 2004 15,893 0 36 US ASTM A255 covers the setup and test method. Timken publishes a great little book of Jominy data. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm Upvote 0 Downvote
ASTM A255 covers the setup and test method. Timken publishes a great little book of Jominy data. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm
Dec 16, 2004 #3 metengr Materials Oct 2, 2003 15,478 0 0 US Another option is SAE J406 specification - Methods for Determining Hardenability of Steels http://www.sae.org/servlets/productDetail?PROD_TYP=STD&PROD_CD=J406_199805 Upvote 0 Downvote
Another option is SAE J406 specification - Methods for Determining Hardenability of Steels http://www.sae.org/servlets/productDetail?PROD_TYP=STD&PROD_CD=J406_199805