Hey All,
I am having a hard time understanding the following code section:
B31.5 - Refrigeration piping
Section - 527.3.2(d)(4)(5) Butt Welds
(d) The welding shall be such as to assure that the following requirements are met:
(4)Incomplete Penetration. The total joint penetration shall not be less than the thinner of the two components being joined, except to the extent that incomplete root penetration is permitted for girth welds only. The depth of incomplete root penetration at the weld root of girth welds shall not exceed 1/32 in. (0.8mm) or one half the thickness of the weld reinforcement, whichever is smaller. The total length of such incomplete root penetration or at the root shall not exceed 1 1/2 in. (38mm) in and 6 in. (152 mm) of weld length.
(5) Lack of Fusion. None Permitted.
The part I am struggling with is where it allows for Incomplete root penetration of 1.5" in 6" of weld, yet in the next sentence say Lack of fusion, None Permitted.
If the root is not tied into one or both sides of a typical pipe "V" groove joint, that is lack of fusion of the root. So how are you allowed up to 1.5" of Lack of Penetration of the root? If the root is not penetrated its not fused??? What am I missing here?
Thanks in advance?
I am having a hard time understanding the following code section:
B31.5 - Refrigeration piping
Section - 527.3.2(d)(4)(5) Butt Welds
(d) The welding shall be such as to assure that the following requirements are met:
(4)Incomplete Penetration. The total joint penetration shall not be less than the thinner of the two components being joined, except to the extent that incomplete root penetration is permitted for girth welds only. The depth of incomplete root penetration at the weld root of girth welds shall not exceed 1/32 in. (0.8mm) or one half the thickness of the weld reinforcement, whichever is smaller. The total length of such incomplete root penetration or at the root shall not exceed 1 1/2 in. (38mm) in and 6 in. (152 mm) of weld length.
(5) Lack of Fusion. None Permitted.
The part I am struggling with is where it allows for Incomplete root penetration of 1.5" in 6" of weld, yet in the next sentence say Lack of fusion, None Permitted.
If the root is not tied into one or both sides of a typical pipe "V" groove joint, that is lack of fusion of the root. So how are you allowed up to 1.5" of Lack of Penetration of the root? If the root is not penetrated its not fused??? What am I missing here?
Thanks in advance?