Hello Seniors!
Reference to my last thread809-473593.I thought to end the previous thread but it had been closed already.
But now I am ending it now with the latest updates regarding the issue.
So we were somewhere near two options.
1>To patch weld all the rivets from inside and then paint application.
2>To remove the roof(newly installed) and replace all the remaining shell courses one by one.
But we went for 2nd option with some changes that we started removing shell course(from 2nd shell course)and installing new plates one by one. We completely welded all the new plates. During all these activities roof and old shell courses were temporarily supported by beams and channels. After completion, hydrotesting was performed and there were no leakage as now the tank has been completely replaced by the new one.
Now client is happy and contractor as well. Win-win situation for all.![[bigsmile] [bigsmile] [bigsmile]](/data/assets/smilies/bigsmile.gif)
Here are some pics of Tank-435 before and after completion.
Hello Seniors!
Reference to my last thread809-473593.I thought to end the previous thread but it had been closed already.
But now I am ending it now with the latest updates regarding the issue.
So we were somewhere near two options.
1>To patch weld all the rivets from inside and then paint application.
2>To remove the roof(newly installed) and replace all the remaining shell courses one by one.
But we went for 2nd option with some changes that we started removing shell course(from 2nd shell course)and installing new plates one by one. We completely welded all the new plates. During all these activities roof and old shell courses were temporarily supported by beams and channels. After completion, hydrotesting was performed and there were no leakage as now the tank has been completely replaced by the new one.
Now client is happy and contractor as well. Win-win situation for all.
![[bigsmile] [bigsmile] [bigsmile]](/data/assets/smilies/bigsmile.gif)
Here are some pics of Tank-435 before and after completion.