I have to specify internal surface protection for a carbon steel filter. The filter is working on a very high pressure (180 barg) and 80 °C temperature and is working with injection water an high percentage of chlorides.
To protect the internal surface I would suggest to use a cladding material like AISI 316 since a very high pressure service is usually not indicated for internal lining like glass flake or other lining material.
Anyway the Enginnering company has suggested the Vendor to use the glass flake. I'm not agree with this decision and my opinion is to go ahead with internal cladding, are you agree?
Thanks for responde.
Bye
To protect the internal surface I would suggest to use a cladding material like AISI 316 since a very high pressure service is usually not indicated for internal lining like glass flake or other lining material.
Anyway the Enginnering company has suggested the Vendor to use the glass flake. I'm not agree with this decision and my opinion is to go ahead with internal cladding, are you agree?
Thanks for responde.
Bye