Feb 23, 2006 #1 21oktobar Automotive Oct 26, 2004 2 YU I'm interesting datasheet for Liten MB 62 and Moplen EP 540. Can’t find information for molding shrinkage (ISO 2577, 294-4) Did anyone know that data.
I'm interesting datasheet for Liten MB 62 and Moplen EP 540. Can’t find information for molding shrinkage (ISO 2577, 294-4) Did anyone know that data.
Feb 23, 2006 #2 Demon3 Materials Jun 6, 2005 1,850 US Try http://www.matweb.com for free data on most polymers. Also the suppliers are always happy to help and much data can be downloaded. If you don't find that exact grade it probably doesn't matter, just use a value for generic PP. Upvote 0 Downvote
Try http://www.matweb.com for free data on most polymers. Also the suppliers are always happy to help and much data can be downloaded. If you don't find that exact grade it probably doesn't matter, just use a value for generic PP.