LITHIUM HYDRIDE vs METAL COMPATIBILITY

Status
Not open for further replies.

karlb

New member
Nov 29, 2001
14
WOULD ANYONE HAVE INFORMATION ABOUT WHAT METALS AND/OR COATINGS THAT CAN BE USED WITH LiH WITHOUT SIGNIFICANT REACTION/CORROSION, ESPECIALLY AT TEMPERATURE. OR IF THERE IS LiH COMPATIBILITY TABLE AVAILABLE SOMEWHERE?

THANKS
 
Replies continue below

Recommended for you

No idea about metals but PTFE is the only plastic I know which is resistant up to 100 °C at least.
 
What about Nickel (and ALL the alloys of Nickel)?