ashaykadam
Mechanical
Hi,
We are having few oversized equipment (Height more than 40 m) where due to logistic constraints many vendor's are proposing that they will fabricate the equipment in shop, perform Hydrotest, cut in two pieces, transport them to site, carry out final weld joint at site and perform Localized Hydrotest using external jacket to check final Field Weld Joint.
ASME Sec. VIII Div. 1 does not provide any such guidelines where Localized Hydrotest using external jacket is allowed to check final Field Weld Joint.
Can anybody provide me information whether this procedure of Hydrotest proposed by vendor is acceptable?
If yes, then on what grounds we can accept this w.r.t. ASME Sec. VIII Div. 1 requirements?
If No, then what can be the alternative to carry out Hydrotest of final Field Weld Joint?
Thanks.
Have a nice day!
Ashay Kadam
Sr. Manager
Mechanical Department
thyssenkrupp Industrial Solutions (India) Private Limited (Formerly Uhde India Private Limited)
We are having few oversized equipment (Height more than 40 m) where due to logistic constraints many vendor's are proposing that they will fabricate the equipment in shop, perform Hydrotest, cut in two pieces, transport them to site, carry out final weld joint at site and perform Localized Hydrotest using external jacket to check final Field Weld Joint.
ASME Sec. VIII Div. 1 does not provide any such guidelines where Localized Hydrotest using external jacket is allowed to check final Field Weld Joint.
Can anybody provide me information whether this procedure of Hydrotest proposed by vendor is acceptable?
If yes, then on what grounds we can accept this w.r.t. ASME Sec. VIII Div. 1 requirements?
If No, then what can be the alternative to carry out Hydrotest of final Field Weld Joint?
Thanks.
Have a nice day!
Ashay Kadam
Sr. Manager
Mechanical Department
thyssenkrupp Industrial Solutions (India) Private Limited (Formerly Uhde India Private Limited)