I have an 0.25" edge crack with it's root at the 1/8" rivet in a hat section longeron. The longeron is in the tail boom of a Bell 212. I have convinced myself that a doubler with a single row of rivets down the length of the flange is adequate because the load is distributed only along the length of the longeron. Is there a standard repair to a longeron?
I am hesitant to start putting rivets into the web to accommodate an L shaped doubler to replace missing structure if there is no perpendicular load.
Suggestions are welcomed.
Sorry I can’t draw a picture, but I tried my best with the keyboard.
_______
|.| |.|
|.| |.|
|.| |.|
|.| |.|
|.| |.|
__
__| |__
I am hesitant to start putting rivets into the web to accommodate an L shaped doubler to replace missing structure if there is no perpendicular load.
Suggestions are welcomed.
Sorry I can’t draw a picture, but I tried my best with the keyboard.
_______
|.| |.|
|.| |.|
|.| |.|
|.| |.|
|.| |.|
__
__| |__