I would appreciate information on the closest EN standards in terms of chemistry and mechanical properties to the following ASTM standards. I realize the equivalence may not be exact particularly in the mechanical certification tests.

The ASTM standards are castings and are:
A 351 grade CF8M
and A 216 grade WCB

Thanks,
 
Replies continue below

Recommended for you

As per ASM Heat Treater's Guide (2nd edition, page 795):
ASTM A351, grade CF8M is type 316 Stainless Steel. The chemical composition is:
0.08% C, 1.50% Mn, 2.00% Si, 9.0 to 12.0 % Ni, 18.0 to 21.0% Cr, 2.0 to 3.0% Mo.

Rao Yallapragada