Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

looking for imformation on material A-81R

Status
Not open for further replies.

edge6179

Structural
Jun 25, 2009
1
COULD SOMEONE TELL ME ANYTHING ABOUT A-81R? I CANT FIND ANYTHING ON IT. AND IAM TRYING TO CROSS REFERANCE IT.IT IS STAMPED ON A FLANGE THAT WAS INSTALLED IN THE EARLY 50'S.
 
Replies continue below

Recommended for you

edge6179;
One other option is to have a portable chemical analysis (or PMI)performed on the flange along with portable hardness testing to type the flange material. This is easy enough to do using a local material test lab that has field testing capability.
 