I am going to drill a 0.5mm diam. hole (In the vertical machining Centre) on a titanium bar(Ti 6Al 4V ELI). Now I am asking for a advise for machining that titanium( Also I need a help for the selection of the drilling tool material to machine the titanium. If you have a knowledge or any experience on this issue, I will be happy for sharing them.